Beskrivelse
HIS and HES's guide rings made of glass fiber-reinforced acetal resin
HIS is the guide ring for rod and HES is the stamp.
This type of guide ring withstands deformation under heavy load when the softening point is near
In the fusion point (operating temperature + 115 ° C)
Material
Glass fiber reinforced acetal resin.
At temperatures higher than + 115 ° C, the material should be glass fiber reinforced polyamide resin.
Technical data
Speed: <0.8 m / s
Temperature: -40 ° C to + 115 ° C
dh9 | D -0 +0,05 | E +0,2 | C |
---|---|---|---|
12,0 | 16,0 | 9,6 | > 3 |
14,0 | 18,0 | 9,6 | > 3 |
16,0 | 20,0 | 9,6 | > 3 |
18,0 | 22,0 | 9,6 | > 3 |
20,0 | 24,0 | 9,6 | > 3 |
20,0 | 25,0 | 5,6 | > 3 |
20,0 | 25,0 | 9,7 | > 3 |
22,0 | 26,0 | 9,6 | > 3 |
22,0 | 27,0 | 5,6 | > 3 |
22,0 | 27,0 | 9,7 | > 3 |
25,0 | 29,0 | 9,6 | > 3 |